Titanium Series |
K2TiO3 |
Quality index(Ⅰ) |
|
Quality index(Ⅱ) |
TiO2 |
≥60-65% |
TiO2 |
≥73-77% |
K2O |
≤25-32% |
K2O |
≤17-22% |
S |
≤0.04% |
S |
≤0.03% |
P |
≤0.04% |
P |
≤0.03% |
Density(200mesh) |
≤0.5% |
Density(200mesh) |
Can be ordered by the customer |
Exterior: |
White or pale yellow powder |
Exterior: |
White or pale yellow powder |
Packing: |
25kg bag |
Packing: |
25kg bag |
Use: |
It can be used in low hydrogen welding rod, altenating current and direct current welding rod, and stainless welding rod, extensively. This product is welcomed by every welding rod factory deeply. |
|
Quality index(Ⅴ) |
|
Quality index(Ⅶ) |
TiO2 |
≥73-77% |
TiO2 |
≥73-77% |
K2O |
≤15-22% |
K2O |
≥5-10% |
S |
≤0.02% |
S |
≤0.02% |
P |
≤0.02% |
P |
≤0.02% |
Fe2O3 |
≤1.5% |
SiO2 |
≤5% |
SiO2 |
≤5% |
K2O+Na2O |
≥18-22% |
ZrO2 |
≤1.5% |
lg-Loss |
≤0.5% |
Al2O3 |
≤1.5% |
Density(80-200mesh) |
≥98%
≤10% |
lg-Loss |
≤0.5% |
Density(80-200mesh) |
≥98%
≤10% |
Exterior: |
Yellowish granular crystals |
Packing: |
25kg bag or drum |
Use: |
Good fluidness and property, low S and P, mainly used for flux-cored wire, meticulous weld is performance. |
Picture: |
 |
<< Order Back >> |
|
|